Guides › Filament temperature chart
Filament temperature chart
Short answer: PLA about 190–220 °C nozzle and 20–60 °C bed, PETG about 230–250 °C and 70–85 °C, ABS and ASA about 230–260 °C and 90–110 °C. Use the range printed on your spool as the real starting point.
Typical print temperatures by material
| Material | Nozzle (°C) | Bed (°C) | Part cooling fan | Enclosure |
|---|---|---|---|---|
| PLA | 190–220 | 20–60 | High (about 100%) | Not needed |
| PETG | 230–250 | 70–85 | Low to medium (about 30–60%) | Optional |
| ABS | 230–260 | 90–110 | Off or very low | Recommended |
| ASA | 240–260 | 90–110 | Off or very low | Recommended |
| TPU | 210–230 | 30–60 | Low to medium | Not needed |
| Nylon (PA) | 240–270 | 70–90 | Off or low | Recommended |
| Polycarbonate (PC) | 260–310 | 100–120 | Off or very low | Needed |
Ranges are typical values and vary by brand, pigment and additives. Silk, high-speed, carbon-fibre-filled and engineering blends each have their own range. The label on the spool or the maker’s datasheet always wins.
How to pick a temperature inside the range
Start in the middle of the range on the spool label. Cooler gives cleaner detail and less stringing; hotter gives stronger layer bonding and lets you print faster, because the plastic melts more easily. Best results are usually found by printing a test: a temperature tower changes the temperature every few millimetres, so you can see where stringing, bridging and layer strength are best.
Why bed temperature matters
The bed keeps the first layers warm enough to stick and prevents the edges from cooling and curling. Materials with high shrinkage, like ABS, ASA and nylon, need a hot bed and often an enclosure. See how to fix warping and the first layer guide.
Temperature and moisture
Wet filament behaves like filament at the wrong temperature: it pops, strings and looks rough. Dry first, then tune temperature. Drying temperatures are on the drying chart.
Temperature and speed
Fast printing needs a hotter nozzle, because plastic has less time to melt as it passes through the hotend. If you raise speed and get under-extrusion, try raising the temperature by 5 to 10 °C or check the limit with the volumetric flow calculator.
Tune temperature for a new spool
- Read the range on the label and set the middle value.
- Dry the spool if it is a moisture-sensitive material such as PETG, nylon or TPU.
- Print a temperature tower across the label range.
- Pick the coolest section that still has strong layers and good bridges.
- Save it as a filament profile named after the brand and colour.
Common mistakes
- Copying one profile for every brand. Pigments and additives change the best temperature by 10 °C or more. Re-tune each brand.
- Raising temperature to fix wet filament. It makes steam and stringing worse. Dry the spool instead.
- Cooling PETG like PLA. Full fan on PETG weakens layer bonding. Use a lower fan speed.
- Printing ABS or ASA in a draught. Cold air makes it warp and crack. Use an enclosure or block the draught.
Troubleshooting
| Symptom | Likely cause | Fix |
|---|---|---|
| Stringing and oozing | Nozzle too hot or wet filament | Dry, then lower temperature 5 °C at a time |
| Layers split or weak | Nozzle too cool | Raise temperature 5 to 10 °C and reduce fan |
| Corners lift off the bed | Bed too cool or draughts | Raise bed temperature, add enclosure |
| Poor bridging and drooping | Too hot or fan too low | Lower temperature, raise fan if the material allows |
FAQ
What is the best temperature for PLA?
Most PLA prints well between about 190 and 220 °C on the nozzle, with a bed between room temperature and 60 °C. Start in the middle of the range on your spool and tune with a temperature tower.
What temperature should I print PETG at?
Typically about 230 to 250 °C on the nozzle and 70 to 85 °C on the bed, with a lower part cooling fan than PLA.
What are the right temperatures for ABS and ASA?
About 230 to 260 °C on the nozzle and 90 to 110 °C on the bed, with the fan off or very low and an enclosure recommended.
Does the bed temperature matter for PLA?
A bed of 50 to 60 °C helps adhesion on most plates, but PLA will often stick fine with a bed at room temperature on a textured plate.
Why does my spool say a different range?
Brands tune their formulas differently. Always follow the spool label or the datasheet over any general chart.
How do I find the best temperature for my printer?
Print a temperature tower with the range from the label and choose the coolest section that still gives strong layers and clean bridges.
Keep reading
- Heat-set insert hole sizes
- How to fix under-extrusion
- How to fix elephant's foot
- PETG vs ABS vs ASA
- PLA vs PETG
Recommended gear
- Filament dryer — Dries while you print. Check max temperature (≥70 °C) if you print nylon.
- Overture High Speed PLA, 1 kg (1.75 mm) — Our default PLA pick: tight ±0.02 mm diameter tolerance and fast-print friendly.
- Overture High Speed PETG, 1 kg — Tougher and more heat-resistant than PLA for functional parts.
Some links are affiliate links. MeshMath earns a commission on purchases made through Overture and Anycubic (via Awin) links, at no extra cost to you. Picks are chosen for usefulness, not paid placement.
Tools for this
E-steps & flow calibration calculator
Calibrate extruder e-steps and flow rate, with the exact M92 G-code to send.
Temperature tower G-code generator
Add temperature changes by height to any sliced G-code file.
Filament drying temperature & time chart
How hot and how long to dry PLA, PETG, TPU, Nylon and more.
Volumetric flow & max speed calculator
Turn layer height, line width and speed into mm³/s, or find the max speed your hotend can handle.