Guides › How to fix under-extrusion
How to fix under-extrusion
Short answer: dry the filament, make sure you are not asking the hotend for more plastic than it can melt, check the temperature, then calibrate flow. If it still fails, look for a partial clog or a slipping extruder.
What under-extrusion looks like
Walls look thin or have gaps between lines, top layers show holes, infill looks stringy, and parts feel weak and fall apart along layers. It can be constant or come and go. Constant under-extrusion usually points to settings (flow, temperature, speed). Intermittent under-extrusion usually points to hardware (clog, tension, tangles) or moisture.
Fix it in this order
- Check the filament path. Make sure the spool can turn freely and the filament is not tangled, kinked or rubbing.
- Dry the filament. Wet filament can bubble and pop at the nozzle. See the drying chart.
- Raise the nozzle temperature 5–10 °C or print a temperature tower. Cool plastic does not melt fast enough to keep up.
- Slow down or lower layer height. Check the flow rate your speed demands with the volumetric flow calculator.
- Calibrate extruder steps and flow. The e-steps and flow calculator gives the numbers.
- Check extruder tension and the drive gear. A worn gear or loose idler slips; a very tight one can grind filament.
- Look for a partial clog. Do a cold pull or clean or replace the nozzle.
- Check retraction. Too much retraction can leave gaps after travel moves. Compare with the retraction calculator.
Is it a speed limit?
Every hotend can melt only so much plastic per second. The flow you ask for is layer height × line width × speed. If that is above what your hotend and filament can do, you get under-extrusion at high speed that disappears when you slow down. Print one test at half speed to check.
flow (mm³/s) = layer height × line width × speed
max speed = max flow ÷ (layer height × line width)FAQ
What causes under-extrusion?
The most common causes are wet filament, a nozzle that is too cool for the speed, a flow demand above what the hotend can melt, a partial clog, and a slipping or badly tensioned extruder.
Why does under-extrusion only happen at high speed?
At high speed the hotend may not be able to melt plastic as fast as the slicer asks for it. Slow down or use a thinner layer, and check with the volumetric flow calculator.
Can wet filament cause under-extrusion?
Yes. Moisture turns to steam in the nozzle, which can bubble and make extrusion uneven. Dry the spool before changing other settings.
How do I know if my nozzle is partly clogged?
Extrusion is weak or uneven even at a safe temperature and slow speed, and pushing filament by hand takes noticeably more force than it used to. A cold pull or a new nozzle usually fixes it.
Should I just increase the flow rate?
Only after the cause is fixed. Raising flow can hide a clog or wet filament and cause bulging corners. Calibrate flow after the hardware and temperature are right.
Keep reading
Recommended gear
- Filament dryer — Dries while you print. Check max temperature (≥70 °C) if you print nylon.
- Hardened / brass nozzle set — Spare nozzles; hardened steel for CF/glow filaments.
- Overture High Speed PLA, 1 kg (1.75 mm) — Our default PLA pick: tight ±0.02 mm diameter tolerance and fast-print friendly.
Some links are affiliate links. MeshMath earns a commission on purchases made through Overture and Anycubic (via Awin) links, at no extra cost to you. Picks are chosen for usefulness, not paid placement.
Tools for this
E-steps & flow calibration calculator
Calibrate extruder e-steps and flow rate, with the exact M92 G-code to send.
Temperature tower G-code generator
Add temperature changes by height to any sliced G-code file.
Filament drying temperature & time chart
How hot and how long to dry PLA, PETG, TPU, Nylon and more.
Volumetric flow & max speed calculator
Turn layer height, line width and speed into mm³/s, or find the max speed your hotend can handle.