Guides › PETG vs ABS vs ASA: which filament should you use?
PETG vs ABS vs ASA: which filament should you use?
Short answer: choose PETG for tough functional parts if you have an open printer. Choose ASA for anything that lives outdoors or in a car. Choose ABS for heat-resistant indoor parts you want to sand, glue or smooth with acetone, as long as you can print it in an enclosure.
Side-by-side
| PETG | ABS | ASA | |
|---|---|---|---|
| Ease of printing | Easy; strings more than PLA | Harder; warps without an enclosure | Harder; similar to ABS |
| Nozzle temperature | 230–250 °C | 230–260 °C | 240–260 °C |
| Bed temperature | 70–85 °C | 95–110 °C | 90–110 °C |
| Glass transition (approx.) | ~80 °C | ~105 °C | ~100 °C |
| UV / outdoor | Fair | Poor; yellows and turns brittle | Excellent; made for outdoor use |
| Toughness | Tough, flexes before breaking | Tough, more rigid | Tough, similar to ABS |
| Warping | Low | High | Moderate to high |
| Smell / fumes | Low | Strong (styrene) | Strong (styrene) |
| Enclosure | Not needed | Strongly recommended | Recommended |
| Acetone smoothing and welding | No | Yes | Yes |
| Moisture sensitivity | Medium | Low to medium | Low to medium |
| Density | 1.27 g/cm³ | 1.04 g/cm³ | 1.07 g/cm³ |
Typical values. Glass transition is a guide to when parts start to soften under load; real heat resistance depends on the brand, load and wall thickness.
PETG: the easy all-rounder
PETG prints on almost any printer without an enclosure, sticks well, barely warps and makes tough parts that bend before they break. It resists water and many household chemicals, so it suits planters, brackets, tool holders and anything in a kitchen or bathroom. Its weak points are heat (it softens at a lower temperature than ABS and ASA), stringing, and sticking too well to smooth PEI.
ABS: heat resistance and easy finishing
ABS is the plastic of LEGO bricks and many appliance housings. It handles more heat than PETG and is easy to sand, drill, glue with acetone and smooth to a gloss with acetone vapour. In return it needs a hot bed, an enclosure and ventilation. It shrinks noticeably as it cools, so large flat parts warp and tall parts can crack along layers if the air around them is cold. Sunlight yellows it and makes it brittle over time.
ASA: ABS that survives the sun
ASA prints and behaves much like ABS but is designed to resist UV and weather, which is why it is used for car mirror housings and outdoor fittings. It is the best of the three for anything permanently outdoors or on a car. It needs similar care to ABS: an enclosure, a hot bed, little or no part cooling, and ventilation. It usually costs a little more than ABS.
Strength: which is strongest?
There is no single winner. PETG tends to flex and survive impacts, ABS and ASA are stiffer, and all three are tougher than PLA. In 3D printed parts, layer bonding, wall count and orientation matter more than the choice between these three. A well-printed PETG part beats a cracked ABS part every time. If a part fails, add walls and print it so the load runs along the layers, not across them. The infill guide explains why walls matter most.
Worked example: the same bracket in all three
A mounting bracket with 40 cm³ of plastic (after infill) uses the same 16.6 m of 1.75 mm filament in every material, because length depends only on volume. Weight is different, because density is different:
| Material | Density | Weight of 40 cm³ |
|---|---|---|
| PETG | 1.27 g/cm³ | 50.8 g |
| ABS | 1.04 g/cm³ | 41.6 g |
| ASA | 1.07 g/cm³ | 42.8 g |
So a kilogram of ABS or ASA makes about 20% more of the same part than a kilogram of PETG. When you compare prices, compare cost per part, not cost per spool. Run your own model through the STL weight calculator with each material selected.
Which one for common jobs
| Job | Best pick | Why |
|---|---|---|
| Garden, balcony, bike or car exterior parts | ASA | UV resistance; ABS yellows and turns brittle in sunlight |
| Car interior (dashboard, vents, phone mounts) | ASA or ABS | Glass transition around 100 °C vs about 80 °C for PETG; a car in summer sun can exceed PETG’s limit |
| Brackets, clips, tool holders indoors | PETG | Tough, low warp, no enclosure needed |
| Snap-fits and living hinges | PETG | Bends before it snaps |
| Enclosures for electronics near heat | ABS or ASA | Higher heat resistance; ABS is easy to sand, glue and smooth |
| Parts you want glossy and seamless | ABS (or ASA) | Acetone vapour smoothing |
| Contact with oils, many cleaners or water | PETG | Good chemical and water resistance |
| Open-frame printer, no enclosure | PETG | ABS and ASA warp and crack without warm, still air |
Print settings side by side
| Setting | PETG | ABS | ASA |
|---|---|---|---|
| Part cooling fan | 30–50% | 0–20%, more for bridges | 0–30%, more for bridges |
| Bed surface | Textured PEI; use glue stick as a release layer on smooth PEI | PEI or glue stick, 100 °C bed | PEI or glue stick, 90–110 °C bed |
| Enclosure | Not needed | Strongly recommended | Recommended |
| Brim for large parts | Rarely | Usually | Often |
| Drying | 60–65 °C, 4–6 h | 60–80 °C, 2–6 h | 60–80 °C, 2–6 h |
| Shrinkage | Low | Moderate; compensate on precise parts | Moderate; compensate on precise parts |
Typical starting ranges; follow your filament’s data sheet and fine-tune temperature with a temperature tower. For exact-size parts in ABS or ASA, measure a test print with the shrinkage compensation calculator.
Fumes and ventilation
ABS and ASA are styrene-based and give off a noticeable smell while printing, along with volatile organic compounds and ultrafine particles. Print them in an enclosure, ideally with a filter or vented to outside, and not in a bedroom or small closed room. PETG produces much less odour, but good ventilation is sensible for any 3D printer.
Common mistakes
- Printing ABS on an open printer in a draughty room. Layers cool unevenly, corners lift and tall parts split along a layer line. Use an enclosure, or choose PETG.
- Running the part fan at 100% on ABS or ASA. It weakens layer bonding and causes cracks. Keep it low except for bridges and overhangs.
- Printing PETG on bare smooth PEI. It can bond so strongly that it tears the sheet. Use textured PEI or a thin layer of glue stick as a release agent.
- Choosing PETG for a dashboard part. It can soften in a hot parked car. ASA is the safer choice.
- Expecting acetone to smooth or glue PETG. It does not. Use CA glue or epoxy for PETG.
Troubleshooting
| Symptom | Material | Fix |
|---|---|---|
| Heavy stringing and blobs | PETG | Dry the spool, lower the temperature 5–10 °C, tune retraction (see the stringing guide) |
| Corners lifting off the bed | ABS, ASA | Enclosure, brim, hotter bed, no drafts (see the warping guide) |
| Cracks between layers on tall parts | ABS, ASA | Fan lower, enclosure warmer, slightly hotter nozzle |
| Part fused to the bed | PETG | Glue stick as a release layer, or textured PEI; let the bed cool fully |
| Rough, bubbly surface | All three | Wet filament; dry it using the drying chart |
FAQ
Is ASA better than ABS?
For outdoor use, yes: ASA resists UV and weathering, while ABS yellows and becomes brittle in sunlight. Indoors they perform similarly. ABS is usually a little cheaper and easier to find.
Can I print ABS or ASA without an enclosure?
Small parts are possible in a warm room with no drafts and a brim, but large or tall parts tend to warp and crack. An enclosure, even a simple cover, makes a big difference. Ventilate either way because of the fumes.
Which filament is best for car parts?
ASA. It handles cabin heat better than PETG, whose glass transition is around 80 °C, and unlike ABS it does not degrade in sunlight.
Is PETG UV resistant?
Moderately. It handles outdoor use better than PLA and ABS, but ASA is the better choice for parts in direct sun for years.
Can PETG be smoothed or glued with acetone?
No. Acetone works on ABS and ASA. For PETG use CA (super) glue or epoxy, and sanding or a heat gun for finishing.
Do I need to dry PETG, ABS and ASA?
PETG absorbs moisture faster and strings badly when wet, so dry it at 60–65 °C. ABS and ASA absorb less but still benefit from drying at 60–80 °C if they pop or look rough.
Keep reading
- PLA vs PETG
- How to fix stringing
- First layer adhesion
- How to fix warping
- Designing parts for 3D printing
Recommended gear
- Overture High Speed PETG, 1 kg — Tougher and more heat-resistant than PLA for functional parts.
- Filament dryer — Dries while you print. Check max temperature (≥70 °C) if you print nylon.
- Textured PEI build plate — Reliable adhesion and easy release; check your printer’s size.
Some links are affiliate links. MeshMath earns a commission on purchases made through Overture and Anycubic (via Awin) links, at no extra cost to you. Picks are chosen for usefulness, not paid placement.
Tools for this
STL weight & filament calculator
Drop an STL to get grams, metres of filament and cost for PLA, PETG, ABS and more.
Temperature tower G-code generator
Add temperature changes by height to any sliced G-code file.
Filament drying temperature & time chart
How hot and how long to dry PLA, PETG, TPU, Nylon and more.
Shrinkage compensation calculator
Measure a test print and get the exact scale % plus the value to type into Orca, Bambu, PrusaSlicer or Cura.